3, wash-and-wear agent:
The colophony that water Chinese ink chooses as a result of printing ink manufacturer in use process differs or machine rotate speed passes fast, may cause water Chinese ink dry rate is slower. Accelerate dry agent to be able to adjust water Chinese ink to do dry speed to achieve printing machine rotate speed to ask, improve manufacturing efficiency, its use scale to be 2 ~ 3% .
4, slow dry agent:
Slow dry agent can be restrained and Chinese ink of slow down water does dry career, rise to defend wet action, prevent printing ink to be in forme perhaps happens on reticulation roller dry, reduce an edition and burnt edition to wait presswork the happening of breakdown, use scale is 1 ~ 2% between.